ferrovanadium production process
Aluminothermic (Thermite) Process:Primary method for high-grade ferrovanadium (50–80% V). Raw Materials: Vanadium pentoxide (V₂O₅) or vanadium-rich slag. Aluminum powder (reducing agent). Iron scrap or iron oxide (to adjust Fe content). Fluxes (e.g., lime, fluorite) to control slag formation.
Process Steps: Mix V₂O₅, aluminum, iron, and fluxes in a refractory-lined reactor. Ignite the reaction (externally triggered). Exothermic reaction generates temperatures up to 2,500°C, reducing V₂O₅ to metallic vanadium. Molten ferrovanadium settles at the bottom, while slag (Al₂O₃, CaO) floats on top. Separate the alloy and cool it into ingots. Advantages: High purity (low carbon, sulfur, and phosphorus).
Suitable for producing FeV80 (80% V) and FeV50 (50% V). Disadvantages: High cost of aluminum and limited scalability for very large batches.
ferrovanadium parameters
|
Trademark |
ZhenAn |
|
Product |
Ferrovanadium |
|
Purity |
50%80% |
|
Color |
Grey with Metallic Luster |
|
Shape |
Lump |
| Grade |
Industrial Grade |
|
MOQ |
Negotiable |

our service
1. We elaborate every product to provide customers with the best service.
2. We have rich experience to provide customers with the best services.
3. We have a professional team, which can well feed customers to solve problems and provide better services.
4. We can provide customized services for our customers, and provide high-quality products for them.
Hot Tags: grey with metallic luster ferro vanadium lump, China grey with metallic luster ferro vanadium lump manufacturers, suppliers, factory, FeV alloy 40%, Vanadium Ferroalloys 60%, ferrovanadium 70 , Industrial Ferrovanadium Solid, Ferro vanadium Master Alloy 50, Ferro vanadium Master Alloy Dark