Standard Classification by Vanadium Content
Ferrovanadium is primarily categorized based on its vanadium percentage, with internationally recognized grades:
| Grade | Vanadium (V) Content | Key Impurities (Max %) | Primary Applications |
|---|---|---|---|
| FeV80 | 78–82% | C: 0.15%, Si: 1.5%, Al: 1.5% | Aerospace alloys, high-speed steels, nuclear reactors |
| FeV60 | 58–65% | C: 0.40%, Si: 2.0%, Al: 2.0% | Tool steels, automotive components |
| FeV50 | 48–55% | C: 0.60%, Si: 2.5%, Al: 2.5% | Structural steels (HSLA), pipelines |
| FeV40 | 35–45% | C: 0.75%, Si: 3.0%, Al: 3.0% | General construction, low-cost reinforcement |
Notes:
FeV80 is the highest-purity grade, essential for critical applications requiring minimal impurities.
Lower grades (e.g., FeV40) prioritize cost-efficiency for bulk steel production.

Classification by Production Method
(1) Aluminothermic Ferrovanadium
Process: Reduction of V₂O₅ (vanadium pentoxide) using aluminum powder and iron scrap.
Characteristics:
Low carbon content (<0.1% in FeV80).
High purity but energy-intensive.
Used for premium grades (FeV80/FeV60).
(2) Silicothermic/Electric Arc Furnace (EAF) Ferrovanadium
Process: Reduction of vanadium slag or oxides using silicon (Si) or carbon (C) in an EAF.
Characteristics:
Higher carbon/silicon residues (e.g., FeV50/FeV40).
Cost-effective for mass production.

Classification by Additives & Microalloys
Ferrovanadium may include trace elements to enhance specific properties:
| Type | Key Additives | Purpose |
|---|---|---|
| Nitrided FeV | 3–6% Nitrogen (N) | Improves grain refinement in HSLA steels |
| High-Al FeV | 4–8% Aluminum (Al) | Enhances deoxidation in steelmaking |
| Low-C FeV | Carbon <0.05% | Critical for ultra-high-strength alloys |
Hot Tags: types of ferro vanadium, China types of ferro vanadium manufacturers, suppliers, factory, FeV80 40%, Vanadium Iron 50, Vanadium Iron 80 , Ferro vanadium Dark, Ferro vanadium Master Alloy powder, Vanadium-oxides