Ferrosilicon Classification: FeSi75, FeSi72 and FeSi65 Compared

Oct 14, 2024

Leave a message

What the 75, 72 and 65 Numbers Mean

Ferrosilicon is an iron-silicon alloy used mainly to add silicon to steel and to bind oxygen during deoxidation. Its commercial classification is built on one number: the silicon content. A designation such as FeSi75 states that the alloy is supplied on a 75% silicon basis, FeSi72 on a 72% basis and FeSi65 on a 65% basis. Everything else in the specification - carbon, sulphur, phosphorus, aluminium and size - is written as a limit that sits on top of that silicon basis.

The practical consequence is that silicon content and residual levels move together. Producing a high-silicon alloy requires a cleaner, hotter reduction process, which also drives carbon, sulphur and phosphorus out of the metal. A lower silicon basis is reached with less reduction energy, and the residual elements that were not fully reduced stay in the alloy. That is why FeSi75 shows the tightest residual window, FeSi72 sits in the middle, and FeSi65 carries the widest one.

Silicon Content and Residual Limits

Designation Si content (%) C (max, %) S (max, %) P (max, %) Al options (max, %)
FeSi75 74.0-80.0 0.10 0.02 0.035 2.0 / 1.5 / 1.0 / 0.5 / 0.1
FeSi72 72.0-80.0 0.15 0.02 0.04 2.0 / 1.5
FeSi65 65.0-72.0 0.20 0.03 0.04 2.0

The figures above are the ranges normally quoted in the export trade and are written on a delivered-weight basis. Aluminium is the element that generates the most sub-grades inside the 75 family: a low-aluminium FeSi75 with a 0.5% or 0.1% aluminium ceiling is a different product from the general-purpose 2.0% aluminium grade, and the tightest aluminium limits are reserved for electrical steel, deep-drawing grades and welding consumables where aluminium residues change the texture or the arc behaviour of the deposit.

FeSi75 in Detail

FeSi75 is the reference grade for high-duty deoxidation and for silicon addition to high-silicon steels. Its combination of a 74.0% minimum silicon content with low carbon, sulphur and phosphorus makes it suitable where the steelmaker cannot tolerate residual pickup. Typical uses are electrical steel, spring steel, stainless melting practice, foundry inoculants and the production of silicon-bearing master alloys. Because the reduction is driven further, energy consumption per tonne and the demand on the reductant are both higher than for the lower grades, and that cost shows up directly in the selling price.

FeSi72 and FeSi65 in Detail

FeSi72: a mid-range grade positioned between the high-purity 75 family and the general 65 grade. It is chosen where a slightly wider carbon, sulphur and phosphorus window is acceptable and where the buyer wants a lower cost per unit of silicon, but still needs more silicon efficiency than the 65 grade delivers. Common duties are plain carbon and low-alloy steel deoxidation and general foundry work.

FeSi65: the general-purpose grade with the widest residual window and the lowest unit cost. It is used for bulk deoxidation of carbon steels, as a silicon carrier in casting practice and as feedstock for silicon-bearing briquettes and blends where the residual specification is set by the downstream process rather than by the alloy itself.

Size Fraction and Packing

Classification is not only chemical. Size fraction decides how the alloy behaves in the ladle: coarse lump dissolves slowly and can sit on the slag if the bath is cold, while fine material dissolves quickly but is prone to loss in the gas stream and to dust generation during handling.

10-100 mm lump: the standard export fraction for furnace and ladle addition.

10-50 mm and 3-10 mm: used where the addition system, such as a wire feeder or a bunker, cannot handle oversized lump.

0-3 mm fines and milled powder: used in briquettes, welding electrode coatings, heavy-media suspension and powder-metallurgy blends.

Packing follows the same logic. One-tonne jumbo bags with a liner are standard for container shipments, 25 kg bags suit smaller consumers and repacking operations, and steel drums or vacuum packing are applied when the buyer wants to exclude moisture pickup during a long sea voyage.

How to Select the Right Grade

Start from the steel specification and identify which residual element actually limits the process.

If carbon, sulphur or phosphorus are tightly controlled, buy FeSi75 and then select the aluminium sub-grade that matches the melting practice.

If the residual window is open, FeSi65 or FeSi72 delivers the same silicon recovery at a lower unit cost.

Match the size fraction to the addition method rather than to habit, because dissolution losses usually cost more than the price difference between two size fractions.

Require a mill analysis certificate for the shipped lot and verify that the silicon basis and residual limits are stated against the same standard and test method.

Frequently Asked Questions

Q: Is FeSi75 simply a purer version of FeSi65?
In effect, yes. Both are iron-silicon alloys, and the difference is the silicon basis and the residual window that comes with it. FeSi75 is produced with a deeper reduction, so carbon, sulphur and phosphorus are lower; FeSi65 is produced with less reduction energy and therefore carries a wider residual specification.

Q: Why do the aluminium sub-grades matter if silicon is the main classification number?
Aluminium is the residual that most often limits a ferrosilicon grade for critical applications. Electrical steel and deep-drawing grades specify low aluminium to avoid harming magnetic properties or forming behaviour, and welding consumables limit it to control the deposit analysis, so the same silicon basis can split into several separately traded products.

Q: Which grade should a steel mill use for deoxidation?
For plain carbon and low-alloy steel the general-purpose FeSi65 or FeSi72 is normally sufficient, because deoxidation only needs silicon to bind oxygen and the residual specification of the steel is loose. Where the steel grade limits carbon, sulphur or phosphorus, FeSi75 is required so that deoxidation does not reintroduce those elements.

Q: How much ferrosilicon is normally added to a heat of steel?
Addition depends on the oxygen content of the bath and the target silicon level in the finished steel, so it is calculated per heat rather than fixed. The recovery rate also matters: coarse lump added early in the tap recovers less silicon than correctly sized material added under controlled conditions, which is why sizing discipline reduces consumption.

Q: Does ferrosilicon absorb moisture during shipment?
Powder and fine fractions can pick up moisture from humid air, which creates handling and safety issues during charging. For long voyages the usual answer is a polyethylene liner in the jumbo bag, or drum packing for the finest fractions, and a shipment plan that avoids prolonged open-air storage at a humid port.

Q: What documents should accompany a ferrosilicon shipment?
A commercial invoice, packing list, bill of lading, certificate of origin and a mill analysis certificate covering silicon, aluminium, carbon, sulphur and phosphorus are the normal set. The analysis certificate should relate to the actual heat or lot shipped, and the size fraction and packing should be stated the same way in both the contract and the shipping documents.