Ferrotungsten For Steelmaking Few70 Few80 Wolfram Iron Ferrotungsten

Nov 22, 2024

Leave a message

China High Purity 70%-80% Ferro Tungsten Blocks

 

70% 80% Ferrotungsten

 

High Temperature Alloy Addition Ferrotungsten

 

Ferro tungsten FeW composition (%)
Grade
W
C
P
S
Si
Mn
Cu
FeW80-A
75-85
0.1
0.03
0.06
0.5
0.25
0.1
FeW80-B
75-85
0.3
0.04
0.07
0.7
0.35
0.12
FeW80-C
75-85
0.4
0.05
0.08
0.7
0.5
0.15
FeW70
≧70
0.8
0.06
0.1
1
0.6
0.18

 


Ferrotungsten agglomeration method. An open electric furnace that can be moved on a track and the upper section of the furnace body can be disassembled is used, and carbon is used as a reducing agent. The mixed charge consisting of tungsten concentrate, asphalt coke (or petroleum coke) and slag-making agent (bauxite) is added to the furnace in batches. The metal smelted in the furnace is generally viscous. As the thickness increases, the lower part gradually solidifies.

 

When the furnace is full, stop the furnace, pull out the furnace body, and remove the upper furnace body to condense the agglomerates. Then take out the agglomerates, crush and refine them; pick out the edges, slag and unqualified parts and return them to the furnace for remelting. The product contains about 80% tungsten and no more than 1% carbon.