Thickness Change Of Graphite Electrode

Dec 13, 2024

Leave a message

Thickness change of graphite electrode
The thickness change of battery pole piece has the following different conditions:

(1) Cold rolled pole piece, after rebound, the thicker the compaction density, the greater the rebound; under the same stress, the greater the elastic mold of the adhesive, the smaller the pole piece maintains rebound, and dryness will cause the rebound of the pole piece.

(2) The pole piece absorbs and the lithium battery electrolyte dissolves, and the pole piece thickness can be increased.

(3) During the battery charging process, due to the change of lattice constant parameters, lithium intercalation causes the electrode level to expand.

The lithium conversion process of graphite anode oxidation of lithium-ion battery and the expansion of anode plate are introduced in detail.

The lithium graphite coin half-cell electrode sheet, and in the expansion process shown in Figure 1, the first release of lithium, such as the lithium-ion battery of graphite virtual beam, the electrode potential decreases, and the thickness of the pole piece gradually increases. The whole process can be divided into several stages?EA, with inserted graphite layers to increase the lithium content (x gradually increases), LixC6 exists in several different phases, Table 1 lists some characteristics of this stage, x represents the molecular content of lithium in LixC6, d is the interval of the graphite layer lattice constant parameters, with the inclusion of lithium, from the graphite phase to 2H connection, when SOC50%, into LiC12, become fully lithiated LiC6, 372mAh theoretical capacity / gram. This change, d-layer spacing gradually increases, resulting in an increase in the thickness of the pole piece.

Graphite Electrode Cost
Graphite Electrode Cost
Graphite Electrode Machining
Graphite Electrode Machining